📌 : For each 0.01% reduction in Carbon, an increase of 0.06% in Manganese is allowed, up to a maximum of 1.35% ( American Piping Products ). Mechanical Properties Tensile Strength 60,000 psi (415 MPa) minimum Yield Strength 35,000 psi (240 MPa) minimum Elongation 22% minimum (standard longitudinal) Hardness 197 HBW maximum 🏗️ Manufacturing and Dimensions
👉
| Property | Value | | :--- | :--- | | | Carbon Steel (Seamless or Welded) | | Temperature Range | -29°C to 425°C (-20°F to 800°F) | | Common Shapes | 45/90/180 Elbows, Tees, Reducers, Caps | | Connection Types | Butt-weld (BW) | | Size Range | NPS 1/8″ to 48″ (DN 6 to 1200) | astm a234 wpb specification pdf
If you open the PDF of the specification and look at the "Chemical Composition" table, you will see the DNA of WPB. It is a Carbon-Manganese steel. 📌 : For each 0